Grade : | 301S81 彈簧用不銹鋼帶 | ||||||
Number: | X7CrNiAl17-7 | ||||||
Classification: | 馬氏體鋼和沉淀硬化鋼-特殊等級 | ||||||
Density: | 7.8 g/cm 3 | ||||||
Standard: | |||||||
EN 10088-2:2005不銹鋼。通用耐腐蝕鋼片/板和帶材交貨技術(shù)條件 | |||||||
EN 10088-3:2005不銹鋼。一般用途耐腐蝕鋼的半成品、棒材、線材、型材和光亮產(chǎn)品的交貨技術(shù)條件 | |||||||
EN 10151:2003彈簧用不銹鋼帶。技術(shù)交付條件 | |||||||
EN 10088-1:2005不銹鋼。不銹鋼清單 | |||||||
EN 10088-5:2009不銹鋼。建筑用耐腐蝕鋼棒材、棒材、線材、型材和光亮產(chǎn)品的交貨技術(shù)條件 | |||||||
EN 10088-4:2009不銹鋼。建筑用耐腐蝕鋼片/板和帶材交貨技術(shù)條件 | |||||||
Equivalent grades: | |||||||
Chemical comb % of steel X7CrNiAl17-7 (301S81 ): EN 10088-2-2005 | |||||||
未經(jīng)買方同意,不得故意將本表中未列出的元素添加到鋼材中,除非對鑄件進(jìn)行精加工。 | |||||||
為了獲得更好的冷變形能力,上限Nimay可提高到8.3% | |||||||
C | Si | Mn | Ni | P | S | Cr | Al |
max 0.09 | max 0.7 | max 1 | 6.5 - 7.8 | max 0.04 | max 0.015 | 16 - 18 | 0.7 - 1.5 |
Mechanical properties of steel X7CrNiAl17-7 (301S81 ) | |||||||
Rm - Tensile strength (MPa) (+AT) | 850-1030 | ||||||
A - Min. elongation at fracture (%) (+AT) | 19 | ||||||
Brinell hardness (HB): (+AT) | 255 | ||||||